Model Number: Shell moulding casting
Brand Name: Kerlimar
Key Specifications/Special Features:
In a heated hardening sand (phenolic resin coated sand) covering the heating to 180 ~ 280 ℃ metal template, make its hardening for thin shell (shell thickness is commonly 6 ~ 12 mm), heating solidification shell again, make the enough strength and stiffness, therefore use two pieces of shell fixture clamping or with resin cement, no sand box can constitute a mold, pouring casting metal template of the heating temperature is 300 ℃ or so commonly, use of molding sand, resin sand, the phenolic resin as binder resin sand.Also can use the above method to make thin shell core made of thin shell core dump method commonly used mold.Manufacturing thin shell core commonly used method.Made of resin sand shell mold or shell core can significantly reduce the amount of used sand, casting outline clear, smooth surface, size accurate, do not need mechanical processing or only a small amount of processing.
Shipping Information:
FOB Port:
Tianjin
Lead Time:
10
-
45
days
Main Export Markets:
- Asia
- Mid East/Africa
- Western Europe